CF8C — Nb-stabilised austenitic stainless steel, cast 347 type

Designation

Grade
CF8C
UNS
J92710
EN designation
≈ 1.4552 (GX5CrNiNb19-11)
Commonly associated designations
347 type
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification.
Standard
ASTM A351/A351M, A743/A743M
Density
≈ 7.75 g/cm³
Usual delivery condition
Solution annealed and quenched

Chemical composition

ElementMass fraction, %
C≤ 0.08
Mn≤ 1.50
Si≤ 2.00
Cr18.0–21.0
Ni9.0–12.0
Nb8 × C – 1.00
Febal.

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
Solution annealed and quenched48520530

Minimum values (or ranges) for separately cast test bars as specified in ASTM A351/A351M, A743/A743M.

Characteristics

Corrosion and oxidation behaviour
Good general corrosion resistance
Weldability
Good with matching filler and standard procedures
Machinability
Moderate; work hardening or built-up edge to be considered
Typical applications
Valves Pumps Food processing Chemical processing General engineering

International cross-reference

SystemDesignationRelationship
EN1.4552 (GX5CrNiNb19-11), EN 10283Similar composition
AISI347 (wrought)Comparable properties

Casting and processing considerations

Castings are normally solution annealed and rapidly cooled to dissolve carbides and restore corrosion resistance. Low-carbon grades are preferred where castings will be welded without subsequent heat treatment. High shrinkage requires adequate feeding of heavy sections; surface finish and pickling or passivation requirements should be agreed in advance.