LOSTWAXTRInvestment CastingRequest a quotation

CA6NM — 13Cr-4Ni low-carbon martensitic stainless steel

Designation

Grade
CA6NM
UNS
J91540
EN designation
≈ 1.4317 (GX4CrNi13-4)
Commonly associated designations
13-4 type (F6NM)
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification.
Standard
ASTM A743/A743M, A487/A487M
Density
≈ 7.70 g/cm³
Usual delivery condition
Quenched (or normalised) and tempered

Chemical composition

ElementMass fraction, %
C≤ 0.06
Mn≤ 1.00
Si≤ 1.00
Cr11.5–14.0
Ni3.5–4.5
Mo0.40–1.0
Febal.

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
Quenched (or normalised) and tempered75555015

Minimum values (or ranges) for separately cast test bars as specified in ASTM A743/A743M.

Characteristics

Corrosion and oxidation behaviour
Moderate resistance: atmosphere, fresh water and mild media
Weldability
Possible with qualified procedure; preheat and/or post-weld heat treatment as specified
Machinability
Good in the appropriate heat-treatment condition
Typical applications
Hydro power Pumps Impellers Valves Energy

International cross-reference

SystemDesignationRelationship
EN1.4317 (GX4CrNi13-4), EN 10283Similar composition
JISSCS6 (G 5121)Similar composition
UNS (wrought)S41500Comparable properties

Casting and processing considerations

Properties depend entirely on correct heat treatment, so the required condition must be stated on the drawing or order. Martensitic grades are crack-sensitive during cooling and welding; preheating and controlled tempering are standard practice. For precipitation-hardening grades, homogenisation before solution treatment is often specified for heavier sections.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.

CA15 CA40 GX4CrNi13-4 (1.4317) CB7Cu-1