CB7Cu-1 — Precipitation-hardening stainless steel, cast 17-4 PH type

Designation

Grade
CB7Cu-1
UNS
J92180
EN designation
≈ 1.4525 (GX5CrNiCu16-4)
Commonly associated designations
17-4 PH® type
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification.
Standard
ASTM A747/A747M
Density
≈ 7.80 g/cm³
Usual delivery condition
Solution treated and precipitation hardened

Chemical composition

ElementMass fraction, %
C≤ 0.07
Mn≤ 0.70
Si≤ 1.00
Cr15.50–17.70
Ni3.60–4.60
Cu2.50–3.20
Nb0.15–0.35
N≤ 0.05
Febal.

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
H900117010005
H102510359659
H115086067010

Minimum values (or ranges) for separately cast test bars as specified in ASTM A747/A747M.

Characteristics

Corrosion and oxidation behaviour
Good general corrosion resistance
Weldability
Possible with qualified procedure; preheat and/or post-weld heat treatment as specified
Machinability
Moderate; work hardening or built-up edge to be considered
Typical applications
Aerospace Pumps Impellers Structural parts General engineering

International cross-reference

SystemDesignationRelationship
EN1.4525 (GX5CrNiCu16-4), EN 10283Similar composition
JISSCS24 (G 5121)Similar composition
UNS (wrought)S17400 (17-4 PH)Comparable properties

Casting and processing considerations

Properties depend entirely on correct heat treatment, so the required condition must be stated on the drawing or order. Martensitic grades are crack-sensitive during cooling and welding; preheating and controlled tempering are standard practice. For precipitation-hardening grades, homogenisation before solution treatment is often specified for heavier sections.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.