Designation
- Grade
- M-35-1
- UNS
- N24135
- EN designation
- —
- Commonly associated designations
- Monel® 400 type
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification. - Standard
- ASTM A494/A494M
- Family
- Nickel-based alloys
- Density
- ≈ 8.80 g/cm³
- Usual delivery condition
- As cast
Chemical composition
| Element | Mass fraction, % |
|---|---|
| C | ≤ 0.35 |
| Mn | ≤ 1.50 |
| Si | ≤ 1.25 |
| Cu | 26.0–33.0 |
| Fe | ≤ 3.50 |
| Nb | ≤ 0.5 |
| Ni | bal. |
Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.
Mechanical properties
| Condition | Tensile strength Rm, min. (MPa) | Yield strength Rp0.2, min. (MPa) | Elongation, min. (%) |
|---|---|---|---|
| As cast | 450 | 170 | 25 |
Minimum values (or ranges) for separately cast test bars as specified in ASTM A494/A494M.
Characteristics
- Corrosion and oxidation behaviour
- Very good resistance in seawater and chloride-bearing media
- Weldability
- Good with matching filler and standard procedures
- Machinability
- Moderate; work hardening or built-up edge to be considered
- Typical applications
- Valves Pumps Marine Chemical processing
International cross-reference
| System | Designation | Relationship |
|---|---|---|
| EN / W.-Nr. | 2.4365 (G-NiCu30Nb) | Comparable properties |
| UNS (wrought) | N04400 (Alloy 400) | Comparable properties |
Casting and processing considerations
Melting practice has a strong influence on quality: reactive elements such as aluminium and titanium in superalloys normally require vacuum melting and pouring, while corrosion-resistant grades are commonly air melted with careful control of carbon and silicon. Corrosion-resistant grades are solution annealed; weld repair and its heat treatment must follow the material specification.
Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.