CZ-100 — Cast commercially pure nickel

Designation

Grade
CZ-100
UNS
N02100
EN designation
—
Commonly associated designations
Nickel 200 type
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification.
Standard
ASTM A494/A494M
Density
≈ 8.80 g/cm³
Usual delivery condition
As cast

Chemical composition

ElementMass fraction, %
C≤ 1.00
Mn≤ 1.50
Si≤ 2.00
Cu≤ 1.25
Fe≤ 3.00
Ni≥ 95.0

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
As cast34512510

Minimum values (or ranges) for separately cast test bars as specified in ASTM A494/A494M.

Characteristics

Corrosion and oxidation behaviour
Very good resistance in seawater and chloride-bearing media
Weldability
Good with matching filler and standard procedures
Machinability
Moderate; work hardening or built-up edge to be considered
Typical applications
Valves Pumps Marine Chemical processing

International cross-reference

SystemDesignationRelationship
UNS (wrought)N02200Comparable properties

Casting and processing considerations

Melting practice has a strong influence on quality: reactive elements such as aluminium and titanium in superalloys normally require vacuum melting and pouring, while corrosion-resistant grades are commonly air melted with careful control of carbon and silicon. Corrosion-resistant grades are solution annealed; weld repair and its heat treatment must follow the material specification.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.

CW-12MW CW-2M CX2MW CW-6M N-7M CW-6MC CU5MCuC M-35-1 CY-40 Alloy 718