LOSTWAXTRInvestment CastingRequest a quotation

CA15 — 12 % Cr martensitic stainless steel, cast 410 type

Designation

Grade
CA15
UNS
J91150
EN designation
≈ 1.4008 (GX7CrNiMo12-1)
Commonly associated designations
410 type
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification.
Standard
ASTM A743/A743M, A217/A217M
Density
≈ 7.61 g/cm³
Usual delivery condition
Quenched (or normalised) and tempered

Chemical composition

ElementMass fraction, %
C≤ 0.15
Mn≤ 1.00
Si≤ 1.50
Cr11.5–14.0
Ni≤ 1.00
Mo≤ 0.50
Febal.

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
Quenched (or normalised) and tempered62045018

Minimum values (or ranges) for separately cast test bars as specified in ASTM A743/A743M.

Characteristics

Corrosion and oxidation behaviour
Moderate resistance: atmosphere, fresh water and mild media
Weldability
Limited; crack-sensitive, welding only by agreement
Machinability
Good in the appropriate heat-treatment condition
Typical applications
Valves Pumps Turbine components General engineering

International cross-reference

SystemDesignationRelationship
EN1.4008 (GX7CrNiMo12-1), EN 10283Comparable properties
JISSCS1 (G 5121)Similar composition
AISI (wrought)410 / UNS S41000Comparable properties

Casting and processing considerations

Properties depend entirely on correct heat treatment, so the required condition must be stated on the drawing or order. Martensitic grades are crack-sensitive during cooling and welding; preheating and controlled tempering are standard practice. For precipitation-hardening grades, homogenisation before solution treatment is often specified for heavier sections.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.