LOSTWAXTRInvestment CastingRequest a quotation

Co-28Cr-6Mo (F75) — Cobalt-chromium-molybdenum casting alloy

Designation

Grade
Co-28Cr-6Mo (F75)
UNS
R30075
EN designation
—
Commonly associated designations
CoCrMo (Stellite® 21 type)
Type designations and trade names are given for orientation only. Trade names are trademarks of their respective owners; the cast grade and its standard remain the specification.
Standard
ASTM F75
Density
≈ 8.30 g/cm³
Usual delivery condition
As agreed per specification

Chemical composition

ElementMass fraction, %
Cr27.0–30.0
Mo5.0–7.0
Ni≤ 0.50
Fe≤ 0.75
C≤ 0.35
Si≤ 1.00
Mn≤ 1.00
Cobal.

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
As cast6554508

Minimum values (or ranges) for separately cast test bars as specified in ASTM F75.

Characteristics

Corrosion and oxidation behaviour
Good general corrosion resistance
Weldability
Limited; crack-sensitive, welding only by agreement
Machinability
Difficult; rigid set-ups, low cutting speeds or grinding
Typical applications
Medical Wear parts Turbine components General engineering

International cross-reference

SystemDesignationRelationship
ISOISO 5832-4 (Co-Cr-Mo casting alloy)Similar composition

Casting and processing considerations

Design the casting so that functional surfaces need grinding only. Carbide-containing wear grades have limited ductility and are sensitive to thermal shock during cooling and finishing. Where a specification for implant alloys is referenced, its additional requirements for melting, testing and documentation apply in full and must be agreed explicitly.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.

Co-Cr-W Alloy 6