C87300 — Silicon bronze

Designation

Grade
C87300
UNS
C87300
EN designation
—
Standard
ASTM B584
Density
≈ 8.36 g/cm³
Usual delivery condition
As cast

Chemical composition

ElementMass fraction, %
Cu≥ 94.0
Si3.5–4.5
Mn0.8–1.5
Zn≤ 0.25
Fe≤ 0.20

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
As cast31012420

Minimum values (or ranges) for separately cast test bars as specified in ASTM B584.

Characteristics

Corrosion and oxidation behaviour
Very good resistance in seawater and chloride-bearing media
Weldability
Good with matching filler and standard procedures
Machinability
Moderate; work hardening or built-up edge to be considered
Typical applications
Marine Valves Architectural hardware Electrical

International cross-reference

Casting and processing considerations

Aluminium bronzes form tenacious oxide films, so turbulence-free filling is essential to avoid oxide inclusions. Leaded alloys are restricted in drinking-water and some regional applications; the applicable regulations should be checked before an alloy is specified. Listed strength values originate from sand-casting specifications and are indicative for investment castings.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.