LOSTWAXTRInvestment CastingRequest a quotation

C95400 — Aluminium bronze

Designation

Grade
C95400
UNS
C95400
EN designation
≈ CC331G (CuAl10Fe2-C)
Standard
ASTM B148
Density
≈ 7.45 g/cm³
Usual delivery condition
As cast

Chemical composition

ElementMass fraction, %
Cu≥ 83.0
Al10.0–11.5
Fe3.0–5.0
Ni≤ 1.5
Mn≤ 0.50

Main elements only. Phosphorus, sulphur and residual-element limits are specified in the standard and are not reproduced here.

Mechanical properties

ConditionTensile strength Rm, min. (MPa)Yield strength Rp0.2, min. (MPa)Elongation, min. (%)
As cast51520512

Minimum values (or ranges) for separately cast test bars as specified in ASTM B148.

Characteristics

Corrosion and oxidation behaviour
Very good resistance in seawater and chloride-bearing media
Weldability
Possible with qualified procedure; preheat and/or post-weld heat treatment as specified
Machinability
Moderate; work hardening or built-up edge to be considered
Typical applications
Wear parts Gears and drives Valves Marine

International cross-reference

SystemDesignationRelationship
ENCC331G (CuAl10Fe2-C), EN 1982Comparable properties

Casting and processing considerations

Aluminium bronzes form tenacious oxide films, so turbulence-free filling is essential to avoid oxide inclusions. Leaded alloys are restricted in drinking-water and some regional applications; the applicable regulations should be checked before an alloy is specified. Listed strength values originate from sand-casting specifications and are indicative for investment castings.

Reference data compiled from the cited standards for orientation. Always work from the current edition of the governing specification; values are not a guaranteed LOSTWAX TR delivery specification.